Secondary grinding is achieved with pebble mills or roller mills, producing a product that is 44 to 149 micrometers ( m) (325 to 100 mesh) in size. Some roller mills are designed to use heated air to dry the material as it is being ground. Hammer mills or steam or compressed airpowered jet mills may be used to produce additional final products.